Without countertop will not do, no kitchen, as this part of the kitchen interior has a number of important functions:
- a work surface to cut and prepare their products;
- It is a zone of placement of equipment and instruments;
- sometimes worktop section can be used instead.
Restoration of veneer tabletops kitchen table
Kitchen worktop tends to wear out over time, may appear in a variety of chips, since a long time subject to numerous mechanical stresses and loads.
Partial restoration of burn on a kitchen worktop before and after
Therefore, it is more often than other furniture components kitchen restore, update and repair in order to return to her attractive appearance.
Table top made of particleboard has a low price, as well as a large selection of a variety of colors and textures
These elements of the kitchen furnishings are made from all sorts of materials: wood, chipboard, stone, plastic, glass.
hpl panel chipboard cladding have a huge number of color options and attract buyers an affordable price
The most common type of copies are made of chipboard, as inexpensive and can withstand high temperature. Alternatively, apart isolated matte and glossy, with a coating of plastic. For their manufacture is used laminated, melamine and laminated chipboard.
Lined Chipboard - glued paper sheet impregnated with resin
For laminated particleboard using the same paper, but of greater thickness, impregnated with melamine resin and secured under pressure
May be damaged worktop from moisture and heat, for it appears excessive friability and other damage. Many are wondering how to repair the kitchen countertop.
Veneered chipboard film afraid of water, suffer from water ends and edges countertop
For the restoration of the worn surface of the kitchen table is often used ceramic tile or mosaic
Very often repair countertops can be made independently without the use of special tools.
Restoration of a table of particle board table top before and after
Content
- 1 Repair of plastic countertops
- 2 Laminated models and their repair
- 3 As refurbish furniture countertop using stroke or wax
- 4 Video: Closing cleavage on chipboard
Repair of plastic countertops
countertop apparatus including laminated plastic hpl
In these models, after long loads are formed on the surface of cracks and chips. Here you need to use a special bonding glue to the plastic caused by a gun.
Special glue for plastic Moment
If the surface is badly damaged, it will approach inexpensive normal superglue or "Moment". If cleavage impressive, it can not do without glue "Titan".
Professional glue titanium cylinder for mounting the gun
To seal the crack, plastic triturated to a fine powder and interfere with the adhesive, and then fill the empty space.
Laminated models and their repair
Additional measures to protect the table-tops made of chipboard - the application of the sealant layer and the installation of protective aluminum slats
Countertop surface coated laminated sheet can swell. That it has acquired original form, you need to:
- conventional heated dryer surface in the deformed place;
- remove the damaged part;
- part where the coating has been damaged, to process the adhesive composition (adhesive);
- after 15 min. Pour the thick mixture of sawdust with adhesive PVA infused for 10 min .;
- compacted with a spatula;
- pulling together the upper and lower surfaces to fill the void, using a spatula.
- let dry day.
After deformation, the upper layer replacing countertops may need at too high temperatures
To the original dimensions in line, you need to make a template from the bar of the same height as the worktop. It is placed in the middle plates 2 and tightening the resulting structure clamps. The resulting press will help to find the density of the mixture and to get rid of adhesive residue.
When you bundle the basics of DSP need to clean the excess with a spatula with a mixture of sawdust and emulsions, pull clamps and allow to dry
Restoration countertop like marble with his own hands
As refurbish furniture countertop using stroke or wax
Partial restoration of the countertop table white oak before and after
There are special restorative compositions with which the furniture perfectly restored.
- Furniture hard wax sealed with dents, chips and scratches. It allows you to buy additional material moisture resistance and resistance to mechanical damage. Before you apply, it melted the lighter. Is then applied and allowed to cool for 3 seconds. Then remove the protruding residue with a knife, and clerical zashlifovyvayut.
Fill dents and scratches recommended in two ways: either by using latex fillers, or by using a composition of an epoxy resin
- With furniture stroke treated fine scratches. Pre shaken bar was applied 2 - 3 times and allowed to dry. Once removed the excess with a soft cloth.
Minor defects can be filled by a stroke
Materials for kitchen furniture restoration
To avoid peeling, blistering of the coating, it is necessary further to process all the component parts. To this layer is applied a waterproof sealant to "weak" places (joints between the sink and the table between the table and the slab and al.), And set aluminum strip. This procedure needs to be undertaken as soon as bought furniture.
Chipboard with aluminum rim are much more spectacular ensures durability of furniture
Restoration of lateral cleavage of chipboard